Macro-scale tensile data on additively manufactured (AM) IN625 in the as-built microstructural condition at room temperature and at different strain rates are provided in this data publication....
Search relevance: 1.00 | Views last month: 9 | Catalog Last Checked: September 10, 2026 at 05:52 PM -
Macro-scale tensile data on additively manufactured (AM) IN625 in the as-built microstructural condition at room temperature and at different strain rates are provided in this data publication....
Search relevance: 1.00 | Views last month: 0 | Catalog Last Checked: October 02, 2026 at 07:52 PM