Found 1 dataset matching filters. (clear all filters)
-
This challenge is a follow-on from AMB2022-01 laser powder bed fusion (PBF-LB) alloy Inconel 718 in the as-built condition (no heat treatment). Eight continuum-but-miniature tensile specimens were...
Search relevance: 1.00 | Views last month: 2 | Catalog Last Checked: August 02, 2025 at 03:56 PM